17-4 PH STAINLESS STEEL

 

ELEMENT

 Wt. %

Cr
Ni
Cu
Cb + Ta
C
Fe

16.5
4
4
0.30
0.03 max
Balance

Typical Mechanical Properties

0.2 %
U.T.S. Y.S.
(ksi) (ksi) Elongation % Hardness
As-Sintered 120 105 10 Rc 20-24
 
Heat Treated
(H-900)
185 160 7 Rc 38-42

 

 